What you have to have:
Results – These can be different based on individual preferences:
Tools:
Directions:
- 1st you will require to noticed/file the sprue off the components
- You can pre buff/ pre polish the star parts which would make cleaning a lot easier soon after soldering
- Applying buff sticks to buff again the solid end heading from coarse to wonderful
- As soon as you have received to fine buff paper you can start out to polish employing luxi compound –blue for initial phase with the calico mop
- There are guide marks on the stage of the star pendant and earrings you want to solder jump rings to
- You can file jump rings with triangular file to give them an angle at the ends so they sit flat against the place of the star
- Apply solder paste the place the guide marks are on the stars
- On the soldering block, force the bounce ring in opposition to the stars manual marks and use tweezers to maintain the bounce ring in put
- Utilizing the hand torch, warmth up the reliable star and after it is commencing to turn colour gradually transfer alongside to the jump ring so it gets to tempreture at very same time until eventually the solder melts and joins the items with each other
- Quench and put it in pickle, rinse after pickling to wash off acids.
- If you didn’t buff and pre polish earlier now you will will need to buff again the cast finish and if you require to take away any further solder
- Polish the piece employing luxi compound – blue for initial phase making use of a calico mop
- Then polish with White luxi compound and a fluffy mop
- For your earrings you can open up up your ear wire and then shut it again jointly
- For the star pendant necklace, dependent on the bail you opt for you can either add it instantly the the soar ring or if demanded you may possibly need to add a further smaller jump ring right before the bail.
- Ultrasonic or clean up off any residual polish and include a chain to the pendant.
Optional: you can either wholly shut your findings by soldering them for the duration of soldering phase 9 or depart the findings semi open and just pushed collectively .